低合金镍钢、耐低温钢焊材料——***AW手工电弧焊
低合金镍钢、耐低温钢焊材料——***AW手工电弧焊焊接法产品名称相当规格规格熔敷金属物理性能之一例熔敷金属化学成份之一例(Wt%)主要用途GB牌号AWS抗拉强度MPa屈服强度MPa延伸度%冲击值J(℃)CSiMnNiMo其它***AW手工电弧焊JN-815C1/JN-816C1E5515-C1W707HE8015-C12.6-5.06145103054(-70)0.0570.440.882.60适合焊接铝净钢及2.5%Ni钢,含镍2.5%在低温-60℃-70℃有优良的冲击值。JN-818C1E5518-C1E8018-C12.6-5.05784803284(-60)0.080.640.982.55适合焊接铝净钢及2.5%Ni钢,含镍2.5%在低温-60℃-70℃有优良的冲击值。JN-815C2/JN-816C2E5515-C2W907NiE8015-C22.6-5.05684703247(-90)0.0670.320.883.3适合焊接LNG贮槽或低温用3.5%Ni钢,含适当合金在-70℃-90℃冲击值优良。JN-818C2E5518-C2E8018-C22.6-5.056847032108(-73)0.070.570.903.4适合焊接LNG贮槽或低温用3.5%Ni钢,含适当合金在-70℃-90℃冲击值优良。JN-815C3/JN-816C3E5515-C3E8015-C32.6-5.055947029118(-45)0.070.620.901.020.21适合焊接ASTMA266、235、236、302,在低温-40℃有优良的冲值。JN-818C3E5518-C3E8018-C32.6-5.05494613498(-50)0.0800.520.880.930.23适合焊接ASTMA266、235、236、302,在低温-40℃有优良的冲值。JN-816GE5516-GE8018-G2.6-5.05684803289(-50)0.0800.471.101.54适合焊接LNG贮槽或低温用铝净钢ASTMA537C1,在-50℃有优良的冲值。JN-715NTBE5015-GW607E7015-G2.6-5.05605502565(-60)0.050.321.300.81Ti≤0.003B≤0.003适合焊接09MnNiNb、E36等低温结构钢,在低温-60℃有优良的冲值。JN-715C2LE5015C2LW107E7015C2L2.6-5.05404203067(-100)0.030.240.843.40.1适合焊接低温结构钢及3.5%Ni钢,含适当合金在-90℃-100℃冲击值优良。)