现代S-308L.16N焊条韩国E308L-16
价格:38.00
现代S-308L.16N焊条韩国E308L-16韩国“现代”(HYUNDAI)药芯焊丝品名AWS型号熔敷金属化学成分(%)熔敷金属力学性能特性与用途CMnSiCrNi其他σ0.2(MPa)σb(MPa)δ(%)IV(J)S-7016.HE70160.080.980.48--49057032-29℃/118低碳钢50kgf级高强钢焊接用低氢型焊条S-7016.LE7016-G0.060.70.4-0.749057031-30℃/160-45℃/130低氢型高韧性焊条,焊接-45℃工作的铝***钢S-7016.LSE7016-G0.061.00.3-0.9Ti:0.02B:0.00249058029-45℃/137-60℃/118极低氢型焊条,焊接低温工作的铝***钢及TMCP钢S-7018.1E7018-10.071.50.5--54061028-46℃/46铁粉低氢型***焊条,焊接桥梁,建筑及低温结构S-8018.GE8018-G0.061.10.5-0.755064027-5℃/140铁粉低氢型***焊条,焊接60kgf级结构,如船舶,桥梁等S-9016.GE9016-G0.071.10.5-0.6Mo:0.25530660295℃/160低氢型焊条,焊接高强钢制成的压力容器、车辆等S-11018.-ME11018-M0.081.450.50.31.85Mo:0.3073083024-51℃/120铁粉低氢型焊条,焊接高强钢结构,如HY80,HY100S-308L.16NE308L-160.020.70.81910-55044焊接18%Cr-8%Ni超低碳不锈钢S-309L.16E309L-160.031.30.72312.5-5604122-12型超低碳不锈钢焊接及异种钢焊接S-309MoL.16E309MoL-160.021.20.823.512.8Mo:2.5-69034用途同S-309L.16,但耐热,耐蚀及抗裂性更好S-316L.16NE316L-160.031.10.819.511.5Mo:2.25-55044焊接18%Cr-12%Ni-Mo超低碳不锈钢(SUS316L)韩国“现代”(HYUNDAI)药芯焊丝品名AWS型号熔敷金属化学成分(%)熔敷金属力学性能保护气体特性与用途CMnSiCrNi其他σ0.2(MPa)σb(MPa)δ(%)IV(J)SuperCored71E71T-1/-1M0.031.450.55--540590260℃/124-18℃/94CO2/Ar+CO220-25%全位置焊,可焊接低碳钢及50kgf级高强钢,船舶,桥梁等SuperCored71HE71T-10.0351.450.50--54058028-20℃/85-30℃/55CO2可大电流焊接,高线能量时冲击韧性仍很好SuperCored71MAGE71T-1M0.051.200.55--52057030-20℃/80Ar+CO220-25%工艺性能优异,可焊接船舶,桥梁等SF-70MXHE70T-10.051.650.55--540620280℃/90CO2金属粉芯焊丝,熔敷效率高,焊结构钢SuperCored70BE71T-5/-5MJ0.061.300.31--45054027-40℃/80CO2/Ar+CO220-25%碱性药芯丝,抗裂性好,低温(-20~-50℃)韧性高SuperCored81-K2E81T1-K20.041.200.40-1.5054062028-40℃/75-60℃/55CO2用于焊接液化气储罐等低温钢结构SuperCored81MAGE81T1-Ni1M0.0451.300.25-0.8553461225.8-40℃/80-50℃/65Ar+CO220-25%低温缺口韧性高,用于油气田管线及海洋平台等SF-70W-0.041.050.450.500.35CU:0.40510580280℃/55CO2用于50kgf级耐候钢焊接SW-308LCoredE308LT1-1/-40.031.200.7019.1010.10-59040-20℃/70CO2/Ar+CO220-25%焊接18%Cr-8%Ni超低碳不锈钢SW-309LCoredE309LT1-1/-40.031.300.7023.012.30-61035-20℃/60CO2/Ar+CO220-25%用于不锈钢与碳钢(或低合金钢)的异种钢焊接SW-316LCoredE316LT1-1/-40.031.200.7018.512.0Mo:2.50-59040-20℃/60CO2/Ar+CO220-25%焊接18%Cr-12%Ni-2%Mo超低碳不锈钢SW-347CoredE347T1-1/-40.041.200.8020.010.0Nb:0.40-63035-20℃/70CO2/Ar+CO220-25%焊接含Ti或Nb的18-8型不锈钢(如321,347型)SuperCored308LE308LTO-1/-40.031.500.6019.59.5-60035-20℃/60CO2/Ar+CO220-25%焊接18-8超低碳不锈钢,适合平、横焊,飞溅小SuperCored316LE316LTO-1/-40.031.300.6018.512.0Mo:2.50-59040-20℃/60CO2/Ar+CO220-25%焊接18-12Mo超低碳不锈钢及异种不锈钢接头)